Preparation of the moon-white glaze by carbothermic reduction of Fe2O3 and SiC

Jianfeng Zhu, Pei Shi ∗, Fen Wang, Ting Zhao
School of Materials Science and Engineering, Shaanxi University of Science & Technology, Xi’an 710021, PR China