Effect of Iron Oxide and Phase Separation on the Color of Blue Jun Ware Glaze

Fen Wang∗, Changan Yang, Jianfeng Zhu, and Ying Lin Shaanxi University of Science and Technology, Xi’an 710021, China

Based on the traditional Jun ware glaze, the imitated Jun ware glazes were prepared by adding iron oxide and introducing phase separation agent apatite through four-angle-method. The effect of iron oxide contents, phase separation and the firing temperature on the color of Jun ware glazes were investigated by a neutral atmosphere experiment, optical microscope and scanning electronic microscope. The results showed that the colorant, mainly Fe2O3, contributed to the Jun ware glaze blue and cyan colors of Jun ware glaze. The light scatter caused by the small droplets in phase separation structure only influenced the shade of the glaze color, intensify or weaken the color, and thus made the glaze perfect and elegant opal visual effects, but was not the origin of general blue or cyan colors of Jun ware glaze. In addition, the firing temperature and the basic glaze composition affected the glaze colors to some extent.

wang2015.pdf (397.8 KB)


This text and all user contributions to the Glazy & the Glazy Wiki are licensed under the Creative Commons Attribution-NonCommercial-ShareAlike 4.0 International; additional terms may apply. By using this site, you agree to the Terms of Use and Privacy Policy.
Ceramic Materials Workshop Mighty Mud Mixer Gasworks NYC