I built a three tiered clay separator and thought I’d share the process with you all. About $30 at Home Depot and an hour to build. Message me if you want more info. I have one already for clay water and decided to build another one for my glazing water. Clean water pours into the orange bucket!

there is a drain on the bottom of the top bucket. Just to keep big chunks from going thru :

See the upturned elbow in the bucket. That just lets water from the top of the bucket over flow :

image