Tom’s Currie Grid calculator: http://demeranville.com/pottery/curriecalc.html
2 Likes
The current todo list:
- Modify the way Kaolin/Silica works so that you can label them with different additives instead. E.g. Zinc for crystalline glazes
- Enable additives that stay constant for all recipes - e.g. cobalt
Long term I’d like to integrate this with the glazy materials database and be able to provide analysis for each grid box on demand.
Let me know if you’re using the calculator and post your feature requests below 